Ferrite Grain Coarsening from Hot Rolled Austenite in ODS Steels
Abstract:
The hot rolling at temperature range of 1100 °C to 862 °C and subsequent air-cooling induce a formation of the coarse ferrite grains in the 9CrODS steels. This coarse ferrite is produced by transformation from the severely hot rolled γ-grains to ferrite. Formation process and mechanism of the transformed coarse ferrite are interpreted in terms of a nucleation, growth and coalescence of the same variant ferrite grains under a variant restriction rule.
Info:
Periodical:
Pages:
514-517
Citation:
Online since:
March 2013