Abstract:

In the current work, the objective of shrinkproof wool was rapidly achieved via the synergetic effect between a protease and its bioenzyme activator, dramatically increasing the reaction rate of protease to wool cuticles. Optimal shrinkproof effect was obtained after the wool fiber sample was processed in the enzymatic solution for 3min at 50°C under the optimized treating condition, i.e, the concentrations of protease and enzyme activator were 1.3g/L and 2.5g/L respectively, with the wet pickup ratio of 130%, the resultant wool sample maintained 82% and 80% of its control sample in terms of tenacity and extension @ break, respectively, which meets the requirements for subsequent processing and applications. Further large-scale protease treatment to wool yarns was performed and the test result for shrinkage rate was-3.01% based on the shrinkproof standard test method of IWS TM31(5A×5), indicating satisfactory wool shrinkproof effect at rapid processing rate (7m/min).

You might also be interested in these eBooks

Info:

Periodical:

Pages:

324-330

Citation:

Online since:

November 2015

Export:

Price:

* - Corresponding Author

[1] Jianqin Tao, Jie Wu, Talk about wool shrink proof technology,J. Journal of guangxi textile science and technology. 01 (2002)46-48.

Google Scholar

[2] Molina R, Espin S.J. P, Yubero F, XPS analysis of down stream plasma treated wool: Influence of the nature of the gas on the surface modification of wool,J. Applied Surface Science. 252 (2005)1417-1429.

DOI: 10.1016/j.apsusc.2005.02.147

Google Scholar

[3] Wojciechowska E, Rom M, Wlochowicz A, The use of Fourier transform-infrared (FTIR) and Raman spectroscopy (FTR) for the investigation of structural changes in wool fibre keratin after enzymatic treatment, [J]. Journal of Molecular Structure. 704 (2004).

DOI: 10.1016/s0022-2860(04)00272-8

Google Scholar

[4] Zhuqing Yu, Shugen Wang, The cutin enzyme role in the whole ecological wool preshrunk, J. Journal of textile. 02(2012)85-88.

Google Scholar

[5] Shengrong Hu. Low concentration of DCCA - protease for wool felting shield finishing, D. Jiangnan university. (2010).

Google Scholar

[6] Lenting H.B. M, Schroeder M, Guebitz G. M, New enzyme-based process direction to prevent wool shrinking without substantial tensile strength loss,J. Biotechnology Letters. 28(2006) 711-716.

DOI: 10.1007/s10529-006-9048-0

Google Scholar