Effect of sintering parameters on physical and mechanical properties of powder injection moulded stainless steel-hydroxyapatite composite
Fig 5
Morphology images of the sintered parts at 61 vol.% powder loading at sintering temperature of (A) 1000°C, (B) 1100°C, (C) 1200°C, and (D) 1300°C for 1 hour.