Article Text

Download PDFPDF
Argon laser suture lysis with different suture materials. An experimental study.
  1. C E Hugkulstone,
  2. A F Spencer and
  3. S A Vernon
  1. Academic Unit of Ophthalmology, University Hospital, Nottingham.

    Abstract

    In an in vitro study, 10/0 nylon was found to require a significantly lower laser energy density to produce suture lysis following a single shot than either 10/0 Dacron or 10/0 prolene. Nylon and Dacron monofilament sutures ruptured at reproducible energy levels without significant observable changes at subthreshold irradiation. Prolene, however, was observed to stretch at energy levels below the lysis threshold, under the standard tension produced by a weight of 0.36 (SD 0.02) g. This feature may be of value when performing laser treatment to trabeculectomy flap sutures in the early postoperative period.

    Statistics from Altmetric.com

    Request Permissions

    If you wish to reuse any or all of this article please use the link below which will take you to the Copyright Clearance Center’s RightsLink service. You will be able to get a quick price and instant permission to reuse the content in many different ways.