Expansion of Cement Mortar Mixing Expansive Agent under Different Curing Conditions and Compressive Strength in Constrained Conditions

Article Preview

Abstract:

The expansion of cement mortar mixing expansive agent under standard curing and membrane curing conditions and compressive strength in constrained conditions are studied in this paper. Results show that the early expansion effect of calcium sulphoaluminate hydrate-calcium hydroxide expansive agent is obvious, mid-to late effect of magnesia expansive agent increase clearly. Compare with standard curing, the shrinkage of the basic cement mortar increase and expansion effect of expansive agent reduce under membrane curing. The expansion effect of expansive agent B is good and persistent under membrane curing, its applicable to used in the closed environment, such as concrete filled steel tubes. The compressive strength of mortar with expansion agent is a little more than the basic mortar under the condition of limit.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

2534-2537

Citation:

Online since:

September 2013

Export:

Price:

* - Corresponding Author

[1] CHEN Li-da, XIE Li-guo, LI Hong-yan, eta1. Further study on basic mechanical of concrete mixed with MgO under different temperature conditions[J]. Guangdong Water Resources and Hydropower, 2003, 4(2): 12-13.

Google Scholar

[2] LI Chen-mu. The influences high content of fly ash on autogenous volume deformation of concrete with MgO[J]. Sichuan Water Power, 2000, 19: 72-75.

Google Scholar

[3] Song Jun-wei, Fang Kun-he. Research and development of hydraulic concrete autogenous volume deformation characteristics[J]. Water Power, 2008, 32(2): 71-74.

Google Scholar

[4] Gao Pei-wei, Lu Xiao-lin, Tang Ming-shu. Shrinkage and expansive strain of concrete with fly ash and expansive material[J]. J Wuhan Univ Technol-Mater Sci, 2009, 24(1): 150-153.

DOI: 10.1007/s11595-009-1150-4

Google Scholar

[5] Xue Yan-li. Cause and prevention of cracking in mass concrete[J]. Cement Technol 2011, 04: 94-95.

Google Scholar

[6] Zheng Jian-lan, Wang Xue-fang. Influence of fly ash on early-age cracking behavior of high-flowing concrete[J]. J Cent South Univ Technol, 2009; 16: 312-319.

DOI: 10.1007/s11771-009-0053-z

Google Scholar

[7] Liu Yu-li, Huang Li-bo, Yang Wei. Analysis on the stress and strain data of Jiangya dam[J]. Dam Safe 2011, 4: 23-27.

Google Scholar

[8] Spingenschmid R. Prevention of thermal cracking in concrete at early ages[J]. London: E&FN Spon, 1998: 1–5.

Google Scholar

[9] OKAMURA H.Physical properties of chemically prestressed concrete[J]. Journal of JSCE, 1974, 226: 101-108.

Google Scholar

[10] OKAMURA H, TSUJI Y, MARUYAMA K. Application of expansive concrete in structural elements[J]. Journal of the Faculty of Engineering, University of Tokyo(B), 1978, 34(3): 48l-507.

Google Scholar

[11] DENG Min, CUI Xue-hua, LIU Yuan-zhan, eta1. Expansive mechanism of magnesia as an additive of cement[J]. Journal of Naniing University of Technology: Natural Science, 1990, 12(4):l-11.

Google Scholar

[12] CUI Xue-hua, LIU Zheng, TANG Ming-shu. Expansion regularity and influencing factors of magnesia-added cement[J]. Journal of Nanjing University of Technology:Natural Science, 1990, 12(4): 20-24.

Google Scholar

[13] LI Cheng-mu. Basic mechanics and long term durability of concrete mixed with MgO[J].Advances in Science and Technology of Water Resources, 2000, 20(5): 30-35.

Google Scholar

[14] QIAN Hal-yan, DENG Min, XU Ling-ling, eta1. Study on the method of determining activity of light-burned magnesia[J]. Industrial Minerals&Processing, 2005, 34(1): 22-24.

Google Scholar