Abstract:

The effectiveness of microalloying addition and two-step aging on the mechanical properties of the Al-Zn-Mg alloy has been investigated using TEM, tensile test and nanoindentation. By decreasing width of PFZ and size of grain boundary precipitates through the addition of (Ag+Sn) or two-step aging process, tensile properties of Al-Zn-Mg alloys are markedly improved. The elongation was quantitatively related to the three microstructural factors; i.e. the width of PFZ, size of grain boundary precipitates and the level of proof stress, to predict ductility of the alloys with known microstructural factors. The fracture mode change is reasonably in terms of the hardness difference between grain interiors and PFZ region by a noindentation technique.

You might also be interested in these eBooks

Info:

Periodical:

Materials Science Forum (Volumes 561-565)

Pages:

235-238

Citation:

Online since:

October 2007

Export:

Price:

[1] For example; G. Thomas and J. Nutting: J. Inst. Metals, Vol. 88 (1959-60), p.81.

Google Scholar

[2] T. Ogura, S. Hirosawa, A. Cerezo and T. Sato: Mater. Sci. Forum, Vol. 519-521 (2006), p.431.

Google Scholar

[3] T. Ogura, S. Hirosawa and T. Sato:J. Japan Inst. of Light Metals, Vol. 56 (2006), p.644. A.Q. 101.

Google Scholar

[10] [2] [10] [3] [0] [50] 100 150 200 Al-Zn-Mg ternary Ag-added Aging time, t / ks Hardness difference, Δ H / mgf/ µm2 Intergranular fracture Transgranular fracture Fig. 4 Relationship between hardness difference and aging time in the Al-Zn-Mg ternary and Ag-added alloys aged at 433K.

DOI: 10.1201/9781351045636-140000172

Google Scholar