Effect of 4-MET- and 10-MDP-based Primers on Resin Bonding to Titanium
Youhei TSUCHIMOTOYasuhiro YOSHIDAAtsushi MINEMariko NAKAMURANorihiro NISHIYAMABart VAN MEERBEEKKazuomi SUZUKITakuo KUBOKI
Author information
Keywords: Titanium, 10-MDP, 4-MET
JOURNAL FREE ACCESS

2006 Volume 25 Issue 1 Pages 120-124

Details
Abstract

The purpose of this study was to investigate the effect of a 4-MET- and 10-MDP-based primer on the bond strength of two resin cements (SuperBond C&B, Sun Medical; Panavia Fluoro Cement, Kuraray) to titanium (Ti). Ti plates were treated with six experimental primers consisting of, respectively, 10-MDP and 4-MET in concentrations of 0.1, 1 and 10wt%, or were kept untreated (control). The highest tensile bond strength of Panavia Fluoro Cement to Ti was obtained when the Ti surface was pre-treated with 10wt% 10-MDP and was significantly higher than that when a lower concentrated 10-MDP-based primer or any 4-MET-based primer was used. On the contrary, no significant difference in tensile bond strength of SuperBond C&B was found for the untreated and six pre-treated Ti surfaces, although pre-treatment with each 10-MDP-based primer resulted in a higher tensile bond strength as compared to any 4-MET pre-treatment. Altogether, the data obtained strongly suggest that 10-MDP is effective to improve the adhesive performance of resin to titanium.

Content from these authors
© 2006 The Japanese Society for Dental Materials and Devices
Previous article Next article
feedback
Top