초록

In this study, effect of MgO/CaO molar ratio on the floor tiles properties was investigated. The viscosity of the bodies wassuccessfully calculated by fleximeter analyses data. High MgO/CaO ratio causes enhancement of the densificationtemperatures and dissolution of the crystals in the floor tile body. The results showed a, during firing, high MgO/CaO ratioup to 6,505 value, formed, low viscosity liquid phase and allowed low sintering temperature approximately 20 oC whencompared to the standard floor tile body. For YK_3 composition will be evaluated due to has allowable deformation amountfor the production. This floor tile composition will be successfully produced in production line.

키워드

Floor tile, Deformation, Viscosity, Sintering

참고문헌(6)open

  1. [단행본] F.H. Norton / 1970 / Fine ceramics: Technology and applications / McGraw Hill : 70 ~ 75

  2. [단행본] A. Dinsdale / 1986 / Pottery science: Materials, Processes and Products / Ellis Horwood Limited : 40 ~ 52

  3. [단행본] W.E. Warrol / 1982 / Ceramic raw materials / Pergamon : 70 ~ 100

  4. [보고서] A. Vari / 2000 / Raw material preparation and forming of ceramic tiles : 45 ~ 60

  5. [학술지] Zahide Bayer Ozturk / 2012 / An investigation of the effect of alkaline oxides on porcelain tiles using factorial design / Journal of Ceramic Processing Research 13 (5) : 635 ~ 640

  6. [학술지] Tuna AYDIN / 2014 / Effect of spodumene addition on pyroplastic deformation of porcelain stoneware / Journal of Ceramic Processing Research 15 (6) : 486 ~ 491