초록

ZrO2/SiC/TiO2 composite ceramics were sintered. These specimens were heat treated at 1073 K and 1173 K for 1, 3 and 10 hrs,and evaluated the mechanical properties and the wear characteristics. The bending strengths of ZST specimens were almostthe same. ZST specimens were able to crack-healing due to addition of SiC, and the strength was increased by addition of TiO2. The Vickers hardness of the as-received ZST specimen was higher than that of the heat treated specimens. The Vickershardness of the heat treated specimens decreased with increasing temperature and time. The coefficient of friction of the ZSTspecimens increased with increasing heat treatment temperature and heat treatment time. The friction coefficients of ZSTspecimens were inversely related to Vickers hardness. The wear loss increased with the heat treatment time at each heattreatment temperature. The wear loss of all specimens was inversely proportional to the Vickers hardness, but the wear losswas proportional to the friction coefficient.

키워드

ZrO2/SiC/TiO2 composite ceramics, Heat treatment, Vickers hardness, Friction coefficient, Wear loss

참고문헌(5)open

  1. [학술지] 남기우 / 2012 / The crack healing behavior of $ZrO2/SiC composite ceramics with $TiO2 additive / Journal of Mechanical Science and Technology 26 (7) : 2093 ~ 2096

  2. [학술지] Sandan Kumar Sharma / 2016 / Tribological Behavior of Silicon Carbide Ceramics - A Review / 한국세라믹학회지 53 (6) : 581 ~ 596

  3. [학술지] Ki Woo Nam / 2012 / Wear characteristics of Si3N4/SiC composite ceramics with added SiO2 colloid / Journal of Ceramic Processing Research 13 (5) : 571 ~ 574

  4. [학술지] 이광호 / 2018 / A study on the wear characteristics of ZrO2 monoliths and ZrO2/SiC composites / Journal of Ceramic Processing Research 19 (1) : 54 ~ 64

  5. [학술지] 남기우 / 2009 / Cracked-healing and the bending strength of Si3N4 composite ceramics with SiO2 additions / Journal of Ceramic Processing Research 10 (4) : 497 ~ 501