粉コークスと気体燃料の併用焼結技術における酸素富化の影響
岩見 友司山本 哲也樋口 隆英主代 晃佐藤 道貴大山 伸幸
著者情報
ジャーナル オープンアクセス HTML

2014 年 100 巻 2 号 p. 189-197

詳細
抄録

The temperature in the sintering bed is preferably maintained between 1200°C and 1400°C during sintering to produce high strength and reducibility sintered ore. To achieve this condition, the technology of combined usage of coke breeze and gaseous fuel, which is fed properly from the top surface of the sintering bed, was developed. In this paper, the effect of oxygen enrichment with combined usage of coke breeze and gaseous fuel on the heat pattern in sintering bed and cold strength of sintered ore was investigated. The cold strength of sintered ore was improved by the oxygen enrichment in the pot test. Then, the holding time over 1200°C during sintering was extended and improvement of strength would be attributed to promotion of the sintering reaction. By the simulation model calculations based on chemical kinetics, it is considered that the further extension of the holding time over 1200°C due to oxygen enrichment is caused of an increase in the distance between the combustion points of the coke breeze and gaseous fuel. However, improvement of the cold strength reached saturation over 32vol.% of the oxygen concentration in suction air. It is also considered that the excessive increase of the distance between the combustion points of coke breeze and gaseous fuel decreases overlap of respective heat transfer and doesn’t contribute to the expansion of holding time over 1200°C.

著者関連情報
© 2014 一般社団法人 日本鉄鋼協会

This article is licensed under a Creative Commons [Attribution-NonCommercial-NoDerivatives 4.0 International] license.
https://creativecommons.org/licenses/by-nc-nd/4.0/
前の記事 次の記事
feedback
Top