Abstract
The aluminum-lithium alloy 2090-T8E41 undergoes delamination along certain high-angle boundaries parallel to the rolling plane when subjected to torsional loading. Weak boundaries were located by comparison of fracture surface replicas and thin foils in the electron microscope. Grain boundary orientation was determined from Kikuchi patterns obtained by convergent beam electron diffraction.
Similar content being viewed by others
References
P. Heilmann, W.A.T. Clark and D.A. Rigney, Ultramicroscopy 9, 365 (1982).
A.K. Vasudévan and R.D. Doherty, Acta Metall. 35 (6), 1193 (1987).
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Crooks, R., Porter, J.R. Orientation of Weak Grain Boundaries in Aluminum-Lithium Alloy 2090-T8E41. MRS Online Proceedings Library 122, 425–427 (1988). https://doi.org/10.1557/PROC-122-425
Published:
Issue Date:
DOI: https://doi.org/10.1557/PROC-122-425