Abstract
The study of polycrystalline CeO2 + xSm2O3 (x = 0, 10.9–15.9 mol %) thin films deposited by Electron Beam Physical Vapour Deposition (EB-PVD) and Ionic Beam Assisted Deposition (IBAD) techniques on the Si substrate was devoted to the influence of deposition conditions used, namely composition x, deposition temperature T dep and Ar+ ion bombardment as well as the structure and (micro)structure on the (micro)hardness H using the differential hardness, Hdif, as a parameter. The investigations were made using, as in our recent papers, the depth sensing indentation (DSI) technique. The study was focused on the depth dependence of the film/substrate system response on the indentation response from the surface of films up to the film/substrate interface. This study has shown that the critical indentation depth, where the influence of substrate is negligible, can be observed for some CeO2 films doped with Sm2O3 as well as for undoped CeO2 films, both deposited at Tdep = 200°C without IBAD as well as using IBAD. Besides it, a wavy character of differential curve due to the inhomogeneities of films was observed with good reproducibility at some films. It was proven, that the method of differential hardness measurement is applicable for the determination of critical indentation depth as well as for the study of microstructure response of thin films from the film surface up to the film/substrate interface. Results of this study are described and discussed.
Similar content being viewed by others
References
Battacharya, A.K. and Nix, W.D., Int. J. Solids Struct., 1988, vol. 24, p. 881.
Battacharya, A.K. and Nix, W.D., Int. J. Solids Struct., 1988, vol. 24, p. 1287.
Oliver, W.C. and Pharr, G.M., J. Mater. Res., 1992, vol. 7, p. 1564.
Saha, R. and Nix, W.D., Acta Materialia, 2002, vol. 50, p. 23.
McGurk, M.R. and Page, T.F., J. Mat. Res., 1999, vol. 14, p. 2283.
Jonson, B. and Hogmark, S., Thin Solid Films, 1984, vol. 114, p. 257.
Burnet, P.J. and Rickerby, D.S., Thin Solid Films, 1987, vol. 148, p. 41.
Bull, S.J. and Rickerby, D., Surf. Coat. Technol., 1990, vol. 42, p. 149.
Chicot, D. and Lessage, J., Thin Solid Films, 1995, vol. 254, p. 123.
Lessage, J., Pertuz, A., Puchi-Cabrera, E.S., and Chicot, D., Thin Solid Films, 2006, vol. 497, p. 232.
Hartmanová, M., Navrátil, V., Buršíková, V., Kun-dracik, F., and Mansilla, C., Russ. J. Electrochem., 2011, vol. 47, pp. 505–516.
Alexopoulos, P.S. and O Sulivan, T.C., Annu. Rev. Mater., 1990, vol. 20, p. 391.
Ahn, J.-H. and Kwon, D., Mater. Sci. Eng., Ser. A, 2000, vol. 285, p. 172.
Jung, Y.-G., Lawn, B.R., Martyniuk, M., Huang, H., and Hu, X.Z., J. Mater. Res., 2004, vol. 19, p. 3076.
Clifford, C.A. and Seah, M.P., Nanotechnol., 2006, vol. 17, p. 5283.
Calabri, L., Mantovani, S., Pettighieri, L., and Valeri, S., Int. J. Mat. Res., 2008, vol. 99, p. 8.
Hartmanová, M., Jergel, M., Mansilla, C., Holgado, J.P., Zemek, J., Jurek, K., and Kundracik, F., Appl. Surf. Sci., 2009, vol. 255, pp. 9085–9091.
Hartmanová, M., Náda dy, V., Kundracik, F., and Mansilla, C., Appl. Surf. Sci., 2013, vol. 269, pp. 65–71.
Buršíková, V., Hartmanová, M., Navrátil, V., and Man-silla, C., Russ. J. Electrochem., 2013, vol. 49, pp. 619–627.
Dennis, J.E., Jr., State of the Art in Numerical Analysis, Jacobs, D., Ed., Academic Press, 1977, pp. 269–312.
Moré, J.J., Numerical analysis, Watson, G.A., Ed., in Lecture Notes in Mathematics, Springer Verlag, 1977, vol. 630, pp. 105–116.
Byrd, R.H., Shnabel, R.B., and Shultz, G.A., Math. Programming, 1994, vol. 67, no. 2, pp. 189–224.
Author information
Authors and Affiliations
Corresponding author
Additional information
Based on the paper presented at the XII Meeting “Fundamental Problems of Solid State Ionics”, Chernogolovka (Russia), July 3–5 2014.
The article is published in the original.
Rights and permissions
About this article
Cite this article
Buršíková, V., Hartmanová, M., Navrátil, V. et al. Influence of deposition conditions on electrical and mechanical properties of Sm2O3-doped CeO2 thin films prepared by EB-PVD (+IBAD) methods. Relationship between investigated film and substrate at indentation. Russ J Electrochem 51, 495–502 (2015). https://doi.org/10.1134/S102319351506004X
Received:
Published:
Issue Date:
DOI: https://doi.org/10.1134/S102319351506004X