Abstract
ALD-clad-pumped nanosecond Tm3+ doped silica fiber amplifier was reported that provided up to a 2-W average power output with a slope efficiency of 48.6% with respect to the absorbed pumped power. The input signal central wavelength was at 1.99 μm, with a 119.5-ns pulse duration and 5-kHz repeat rates. The pump sources were a 793-nm LD output with a 400-μm pigtail fiber. The gain fiber was D-shaped Tm3+ doped silica double-clad fiber with a diameter of 27.5/400 μm. The output amplified pulse and spectrum were in accordance with the input signal. This is the first report to the authors’ knowledge on the general experimental investigation of a LD-clad-pumped Tm3+ doped silica nanosecond-fiber amplifier at 1.99 μm.
Similar content being viewed by others
References
G. P. Frith and D. G. Lancaster, Proc. SPIE 5620, 36 (2004).
G. P. Frith and D. G. Lancaster, Proc. SPIE 6102, 610208-1 (2006).
X. M. Duan, B. Q. Yao, Y. J. Zhang, and C. W. Song, Laser Phys. Lett. 5, 347 (2008).
Y. F. Li, Y. Z. Wang, and B. Q. Yao, Laser Phys. Lett. 5, 37 (2008).
M. Meleshkevich, N. Platonov, D. Gapontsev, and A. Drozhzhin, Cleourope, IQEC2007, CP2-3-THU (2007).
E. Marc, Opt. Lett. 30, 456 (2005).
E. Marc, Opt. Lett. 30, 3329 (2005).
M. Meleshkevich, A. Drozhzhin, and N. Platonov, Proc. SPIE 5709, 117 (2005).
G. Imeshev and M. E. Fermann, Opt. Express 13, 7424 (2005).
J. Limpert, S. Hofer, A. Liem, and H. Zellmer, Appl. Phys. B 75, 477 (2002).
L. F. Kong, Q. H. Lou, and J. Zhou, Opt. Eng. 45, 010502-1 (2006).
A. Liem, J. Limpert, H. Zellmer, and A. Tünnermann, Opt. Lett. 28, 1537 (2003).
Author information
Authors and Affiliations
Corresponding author
Additional information
Original Text © Astro, Ltd.
Rights and permissions
About this article
Cite this article
Tao, J., Yunjun, Z. & Hanbin, W. LD-clad-pumped nanosecond Tm3+ doped silica fiber amplifier at 1.99 μm. Laser Phys. 18, 996–998 (2008). https://doi.org/10.1134/S1054660X0808015X
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1134/S1054660X0808015X