Area Ratio of Cathode/Anode Effect on the Galvanic Corrosion of High Potential Difference Coupling in Seawater

, and

Published under licence by IOP Publishing Ltd
, , Citation Zhijian Wang et al 2018 IOP Conf. Ser.: Mater. Sci. Eng. 322 022046 DOI 10.1088/1757-899X/322/2/022046

1757-899X/322/2/022046

Abstract

The galvanic corrosion behaviours of copper nickel alloy(B10)/low-alloy high strength steel(921A) and commercially pure titanium(TA2)/low-alloy high strength steel (921A) was studied by electrochemical method in seawater with different cathode/anode area ratio(Sc/Sa). Results indicated that 921A is the anode and B10 and TA2 is the cathodes. The Sc/Sa has a significant impact on the galvanic corrosion, galvanic corrosion rate of high potential difference coupling showed linear growth with the Sc/Sa, but had extreme because the galvanic potential shift and driving voltage decreases.

Export citation and abstract BibTeX RIS

Content from this work may be used under the terms of the Creative Commons Attribution 3.0 licence. Any further distribution of this work must maintain attribution to the author(s) and the title of the work, journal citation and DOI.

Please wait… references are loading.