Abstract
A reflectivity of 45% of the self-pumped phase-conjugate wave in (K0.5-Na0.5)0.2(Sr0.75Ba0.25)0.9Nb2O6:Cu crystal at the environmental temperature T ∼ 70°C has been obtained. The temperature effect in this kind of self-pumped phase-conjugator is studied.