Issue 12, 2003

Control of single crystal morphology of SBA-1 mesoporous silica

Abstract

SBA-1 mesoporous silica has been synthesized in different crystal shapes from C18TMACl–sodium silicate–H2SO4H2O at pH values between 1.0 and 2.0.

Graphical abstract: Control of single crystal morphology of SBA-1 mesoporous silica

Article information

Article type
Communication
Submitted
10 Oct 2003
Accepted
20 Oct 2003
First published
31 Oct 2003

J. Mater. Chem., 2003,13, 2853-2854

Control of single crystal morphology of SBA-1 mesoporous silica

M. Chao, D. Wang, H. Lin and C. Mou, J. Mater. Chem., 2003, 13, 2853 DOI: 10.1039/B313028M

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements