Taking the Stress out of Styrene

Annealing Polystyrene Plastics Parts Requires a Simple but Specific Technique. Controlled-Cycle Water Baths and Fixed-Temperature Ovens are Practical if Results are Checked By the Kerosine Test

00
Scientific American Magazine Vol 176 Issue 1This article was originally published with the title “Taking the Stress out of Styrene” in Scientific American Magazine Vol. 176 No. 1 (), p. 11