Conclusions
In the work described, lanthanum hexaboride single crystals were grown and refined by the levitation zone melting technique with induction heating. The amounts and character of distribution of impurities in the starting and zone-melted materials were determined by quantitative spectral analysis. It is shown that zone melting effectively purifies a starting lanthanum hexaboride powder from many contaminants. The effectiveness of removal of some low-melting-point and volatile elements is increased by their evaporation and escape in the gaseous form from the molten zone. Estimated values of effective coefficients of distribution of many impurities are given.
Similar content being viewed by others
Literature cited
S. V. Ermakov, F. G. Mamedov, P. N. Meerson, and B. M. Tsarev, "Investigation of the emission properties of powdered lanthanum hexaboride as a function of compositin and purity," Izv. Akad. Nauk SSSR, Neorg. Mater.,3, No. 5, 808–812 (1967).
O. K. Nazarenko, V. E. Lokshin, K. S. Akop'yants, et al., "Stability of lanthanum hexaboride cathode operation in welding electron guns," Avtomat. Svarka, No. 6 (255), 50–52 (1974).
J. D. Verhoeven, E. D. Gibson, M. A. Noack, and R. J. Conzemius, "An arc floating zone technique for preparing single crystal lanthanum hexaboride," J. Crystal Growth,36, 115–120 (1976).
T. Tanaka, E. Bannai, and S. Kawai, "Growth of high purity LaB6 single crystal by multifloat zone passage," J. Crystal Growth,30, 193–197 (1975).
K. Tanagi and M. Ishii, "Growth of LaB6 single crystal by a laser heated floating zone method," J. Crystal Growth,40, 1–5 (1977).
Yu. B. Paderno, V. I. Lazorenko, and A. V. Kovalev, "Zone refining and growth of lanthanum hexaboride single crystals," Poroshk. Metall., No. 10, 60–65 (1981).
W. Pfann, Zone Melting [Russian translation], Mir, Moscow (1970).
Author information
Authors and Affiliations
Additional information
Translated from Poroshkovaya Metallurgiya, No. 1 (241), pp. 56–60, January, 1983.
Rights and permissions
About this article
Cite this article
Paderno, Y.B., Lazorenko, V.I., Buryak, N.I. et al. Amounts and character of distribution of impurities in zone-melted single-crystal lanthanum hexaboride. Powder Metall Met Ceram 22, 50–53 (1983). https://doi.org/10.1007/BF00792514