Abstract
This work reports the outdoor weathering performance of ultraviolet (UV)-stabilized polypropylene (PP) products (using PP resins from Saudi Basic Industries Corporation [SABIC]). Different hindered amine light stabilizers (HALS) were used to stabilize PP-film-based formulations that were exposed for 10 months in harsh outdoor weather of Dhahran, Saudi Arabia. Characterization of the exposed PP film products was done in terms of mechanical and Fourier transform infrared (FTIR) spectroscopic properties. HALS are a very effective light stabilizer for polyolefins.[14–16] They do not act by absorbing UV radiation, but by inhibiting degradation of the polymer, which has started the formation of free radicals. They function by scavenging radicals. HALS has low volatility and high extraction resistance. The effectiveness of HALS is independent of product thickness. Another advantage is that it provides a significant level of stabilization at relatively low concentration.[18] Some important types of high molecular weight HALS are Chimassorb 944 and Tinuvin 622, and a low molecular weight HALS is Tinuvin 770. These HALS, together with other UV stabilizers, are commonly used in polyolefin stabilization. The PP film formulations were divided into five categories based on the type of HALS incorporated. This was done to derive meaningful comparison of the various film formulations. The characterization data are presented for an exposure period of 10 months. The unstabilized PP films were degraded within 2.5 months of the exposure period. The performance in terms of decrease in mechanical properties and FTIR spectroscopic properties was assessed as a result of natural weathering for UV-stabilized samples. Following outdoor weathering trials, the lifetimes of certain formulations were determined. On the basis of the FTIR spectroscopic properties, it was determined that generally, the HALS-stabilized PP film formulations delayed the formation of oxidation products including esters, carbonyls, and trans-vinylenes.
Similar content being viewed by others
References
K.S. Minsker, S.V. Kvolesov, and G.E. Zaikov: Degradation and Stabilization of Vinyl Chloride Based Polymers, Pergamon Press, Oxford, 1998.
J. Wypych: Weathering Handbook, Chemtec Publishing Co., New York, 1989.
S.H. Hamid and I. Hussain: “Lifetime Prediction of Plastics” in Handbook of Polymer Degradation, S.H. Hamid, ed., Marcel Dekker, New York, 2000, pp. 699–726.
G. Scott, ed.: Mechanism of Polymer Degradation and Stabilization, Elsevier Applied Science, New York, 1990.
R. Gachter and H. Muller: Plastic Additives, 3rd ed., Hanser, Munich, 1990.
P.P. Klemchuk, ed.: Polymer Stabilization and Degradation, American Chemical Society Symposium Series 280, ACS, Washington, DC, 1985.
N.S. Allen, ed.: “Photostability of Polyolefins” in Degradation and Stabilization of Polyolefins, Applied Science, London, 1983, pp. 283–335.
S.H. Hamid, M.B. Amin, J.H. Khan, A.G. Maadhah, and A.M. Al-Jarallah: “Lifetime of Agricultural Plastics in Harsh Climate” in Proceedings of the American Chemical Society, Division of PMSE, Spring Meeting, Atlanta, GA, 1991, 64, p. 165.
N. Bensemra, T.V. Hoang, and A. Guyot: “Thermal Dehydrochlorination and Stabilization of Polyvinyl Chloride in Solution: Part VI—Dihydropridine as Organic Costabilizer with Zn-Ca Stearates,” Polym. Degrad. Stab., 1990, 29, p. 175.
V.B. Yakovlov, N.I. Litsov, V.I. Nikolaevskaya, and V.K. Skubin: “Chemical Modification of PE Film Stabilized by a Synergistic Mixture of Antioxidants,” Int. Polym. Sci. Technol., 1990, 17(3), p. 47.
F. Gugumus: “Contribution to the Photolysis of Hydroperoxide in Polyethylene,” Polym. Degrad. Stab., 1990, 27, pp. 19–34.
Z. Osawa: “Role of Metals and Metal Deactivators in Polymer Degradation,” Polym. Degrad. Stab., 1988, 20, p. 203.
P. Gijsman, J. Hennekens, and K. Janssen: “Comparison of UV Degradation of Polyethylene in Accelerated Test and Sunlight” in Polymer Durability, ACS Symposium No. 249, Washington, DC, 1996, pp. 621–36.
J. Malik, A. Hrivik, and E. Tomova: “Diffusion of HALS in Low Density PE and i-PP,” Polym. Degrad. Stab., 1992, 35, pp. 61–6.
F. Gugumus: “Current Trends in Mode of Action of HALS,” Polym. Degrad. Stab., 1993, 40, pp. 165–215.
J.H. Khan and H. Hamid: “Durability of HALS Stabilized PE Film in a Greenhouse Environment,” Polym. Degrad. Stab., 1995, 48, pp. 137–42.
Ciba Geigy Publication No. 28 235/edf. Basel, Switzerland, 1985.
M. Felix and E. Pedrazzetti: “Aspects of LLDPE Stabilization,” presented at European World Perspectives and Development, Ciba Marketing Letter No. 152, Basel, Switzerland, 1986.
C. Zang, D.J. Carlson, and D.M. Wiles: “Hindered Amine Light Stabilizers: Effects of Acid Exposure,” J. Polym. Sci. Part C: Polym. Lett., 1986, 24, p. 453.
A.J. Chirinos-Padron and Allen NS: “Aspects of Polymer Stabilization” in Handbook of Polymer Degradation, S.H. Hamid, M.B. Amin, and A.G. Maadhah, ed., Marcel Dekker, New York, 1992.
N.S. Allen, K.O. Fatinikun, and T.J. Henman: “Thermal and Photochemical Oxidation of Polypropylene,” Eur. Polym. J., 1983, 19(7), pp. 551–54.
G. Geuskens and G. Nedelkos: “The Oxidation of HALS to Nitroxy Radicals in Solution and in Polymers,” Polym. Degrad. Stab., 1987, 19, pp. 365–78.
R. Baumhardt-Neto and A. De Paoli Marco: “Mechanical Degradation of PP: Effects of UV-Radiation,” Polym. Degrad. Stab., 1993, 40, pp. 59–64.
N.S. Allen: “Current Understanding of Photostabilizing Mechanisms in Polyolefins” in New Trends in the Photochemistry of Polymers, N.S. Allen and J.F. Rabek, ed., Elsevier, London, 1986, pp. 209–26.
ASTM D 1435, Outdoor Weathering of Plastics, ASTM, Philadelphia, PA, 1985, 8.01.
ASTM D 882, Tensile Properties of Thin Plastic Sheeting, ASTM, Philadelphia, PA, 1992, 8.01.
R. Mani, N. Sarkar, R.P. Singh, and S. Sivaram, “Surface-Anchored HALS Stabilizers for Improved UV Stability of Polyolefins,” J. Macromol. Sci., Pure Appl. Chem. 1996, A33(9), pp. 1217–26.
D.K.C. Hodgeman: “HALS—Their Role in the Photooxidation of Polypropylene” in Developments in Polymer Degradation, 4, N. Grassie, ed., Applied Science, London, 1982, pp. 189–234.
P. Gigsman and A. Dozeman: “Comparison of UV-Degradation Chemistry of Unstabilized and HALS Stabilized PE & PP,” Polym. Degrad. Stab., 1996, 53, pp. 45–50.
ASTM D 882, Tensile Property of Thin Plastic Sheeting, ASTM, Philadelphia, PA, 1990, 8.01.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Hussain, I., Redhwi, H.H. Development of polypropylene-based ultraviolet-stabilized formulations for harsh environments. J. of Materi Eng and Perform 11, 317–321 (2002). https://doi.org/10.1361/105994902770344141
Received:
Revised:
Published:
Issue Date: