Abstract

The development work for producing an automobile component by thixocasting using A356.2 alloy was introduced. As the first step, the alloy was electromagnetically stirred and solidified to produce a billet with non-dendritic microstructure. The microstructure depended on several process parameters such as stirring intensity, stirring frequency, cooling rate, and melt initial superheat. Through a series of computational studies and controlled experiments, a set of process parameters were identified to produce the best microstructures. Reheating of a billet with non-dendritic microstructure to a semisolid temperature was the next step for thixo-casting of the components. The reheating process was characterized for various reheating cycles using a vertical-type reheating machine. The induction heating cycle was optimized to obtain a near-uniform temperature distribution in radial as well as axial direction of the billet, and the heating was continued until the liquid fraction reached about 50%. These parameters were determined with the help of a computational fluid dynamics (CFD) model of die filling and solidification of the semisolid alloy. The heated billets were subsequently thixo-cast into automobile components using a real-time controlled die casting machine. The results show that the castings are near net shape, free from porosity, good surface finish and have superior mechanical properties compared to those produced by conventional die casting processes using the same alloy.

Cited by (12)

  • Studies on die filling of A356 Al alloy and development of a steering knuckle component using rheo pressure die casting system

    2019, Journal of Materials Processing Technology
    Citation Excerpt :

    In a concurrent study, Guanglei et al. (2010) have used the Carreau model to define viscosity of the semi solid AZ91D Mg alloy slurry, while studying the filling behaviour of connecting rod cavity. In an interesting study performed by Lakshmi et al. (2010), die filling and solidification studies has been discussed in the context of development of automobile components through TDC route using A356 alloy. Improved surface finish and superior mechanical properties compared to those of conventional die cast parts are reported.

  • Modification of microstructure and superficial properties of A356 and A356/10%SiCp by Selective Laser Surface Melting (SLSM)

    2017, Surface and Coatings Technology
    Citation Excerpt :

    Heat treatments, as well as Physical Vapor Deposition (PVD), Chemical Vapor Deposition (CVD), plasma spray and thermal spray coatings have been used to improve the hardness and corrosion, wear, and fatigue resistance of these composites [6,7]. In the last few years, there has been a growing interest in the use of laser techniques to improve the mechanical and tribological properties of light alloys, and techniques such as Laser Surface Melting, Laser Cladding and Surface Alloying have been applied to modify their surface properties leaving the bulk unaffected [8–14]. Laser Surface Melting (LSM) is a well-established technology applied to many materials for hardening, reducing porosity and increasing corrosion resistance.

  • Microstructure characteristics and tensile property of ultrasonic treated-thixocast A356 alloy

    2015, Transactions of Nonferrous Metals Society of China (English Edition)
  • Microstructure and mechanical properties evolution of 6061 aluminum alloy formed by forward thixoextrusion process

    2013, Materials and Design
    Citation Excerpt :

    After obtaining the desired microstructure, the alloy is reheated to the solid and liquid two phase regions and then the billet is forward extruded. There are some effective parameters influencing the semisolid deformation process including solid fraction, holding time in the two phase regions, deformation speed and thermal exchange between material and tool [7]. In this paper, thixoforming process for 6061 wrought aluminum alloy, which is typically used in aircraft structural parts, was investigated.

  • Determination of Optimum Process Parameters and Residual Stress in Friction Welding of Thixocast A356 Aluminum Alloy

    2020, Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science
View all citing articles on Scopus
View full text